Effect of Induction Frequency of Chemical Liquid Vaporization Deposition on Preparation of Hydroxyapatite Coating on C/C composites

机译:化学液体汽相沉积诱导频率对C / C复合材料制备羟基磷灰石涂层的影响

获取原文
获取原文并翻译 | 示例

摘要

Chemical liquid vaporization deposition (CLVD) is used on C/C composites to prepare hydroxyapatite (HA) coating. The induction heating frequencies of CLVD are 450, 390, 330, and 290 kHz. The phase, morphology, and composition of the coatings are characterized by SEM, XRD, and EDS. Adhesion of the coatings onto the C/C substrates is evaluated through a scratch test. Results demonstrate that the induction heating frequencies of CLVD hardly influence the phase of HA coating. With increased induction heating frequency, the critical load increases but the density of HA coating decreases. Under extremely high frequencies, abundant defects are observed on the HA coating surfaces, and the critical load dramatically decreases. The critical load reaches the maximum (47.8 N) at 330 kHz.
机译:在C / C复合材料上使用化学液体汽化沉积(CLVD)制备羟基磷灰石(HA)涂层。 CLVD的感应加热频率为450、390、330和290 kHz。涂层的相,形态和组成用SEM,XRD和EDS表征。通过划痕测试评估涂层在C / C基材上的附着力。结果表明,CLVD的感应加热频率几乎不会影响HA涂层的相。随着感应加热频率的增加,临界负载增加,但HA涂层的密度降低。在极高的频率下,在HA涂层表面观察到大量缺陷,并且临界载荷急剧降低。临界负载在330 kHz时达到最大值(47.8 N)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号