Fillet cracking of no-flow underfill in a flipchip device during a reliability test such as thermal shock or thermal cycling has been a serious reliability problem. The effect of toughening agents and modification of epoxy on fillet cracking of no-flow underfill was investigated. The best epoxy formulation and the appropriate loading level of toughening agent regarding the antifillet cracking performance were found. In the case where the epoxy was modified with polysiloxanes, the second-phase particle with a submicron particle size was formed and the size of the particle depended on the kind of toughening agent. The morphology was observed by a scanning electron microscopy and confirmed by a dynamic mechanical analyzer measurement. The physical properties such as the fracture toughness, flexual modulus, coefficient of thermal expansion, and adhesion were measured, and the liquid-liquid thermal shock (LLTS) test under -55 to 125degreesC was performed with different formulations. One of the formulations toughened by amine/epoxy-terminated polysiloxane, which has higher die shear strength, lower modulus, and higher toughness, passed 1000 cycles of the LLTS test. In order to obtain a high reliable no-flow underfill, the physical properties of the no-flow underfill should be well controlled and balanced. Finally, a correlation between physical properties of the no-flow underfill and the fillet cracking capability for those approaches was discussed. (C) 2003 Wiley Periodicals, Inc. [References: 21]
机译:在可靠性测试(例如热冲击或热循环)期间,倒装芯片器件中的非流动性底部填充材料的圆角开裂已成为严重的可靠性问题。研究了增韧剂和环氧树脂的改性对无流动底部填充胶填角裂缝的影响。找到了最佳的环氧树脂配方和有关抗倒角裂化性能的增韧剂的适当添加量。在用聚硅氧烷改性环氧树脂的情况下,形成具有亚微米粒度的第二相颗粒,并且该颗粒的尺寸取决于增韧剂的种类。通过扫描电子显微镜观察形态,并通过动态机械分析仪测量证实。测量了断裂韧性,挠曲模量,热膨胀系数和粘附性等物理性质,并在不同的配方下于-55至125℃下进行了液-液热冲击(LLTS)测试。其中一种具有较高模切强度,较低模量和较高韧性的用胺/环氧封端的聚硅氧烷增韧的配方已通过LLTS测试1000次循环。为了获得高度可靠的不流动底部填充胶,应很好地控制和平衡不流动底部填充胶的物理性能。最后,讨论了非流动底部填充物的物理性质与这些方法的圆角开裂能力之间的相关性。 (C)2003 Wiley Periodicals,Inc. [参考:21]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号