Modification of epoxy resin with alpha,omega-oligo(butylmethacrylate)diols

机译:用α,ω-低聚(甲基丙烯酸丁酯)二醇改性环氧树脂

获取原文
获取原文并翻译 | 示例

摘要

Novel Liquid rubbers based on bishydroxy-terminated oligo(butylmethacrylate) were used to toughen anhydride-cured epoxy resins. Concentration and molecular weight of the toughening agents were varied in order to examine the effects on important mechanical properties, such as toughness, strength, stiffness, and glass transition temperature. Experimental data show that telechelic methacrylates are suitable toughening agents for epoxies. The compatibility between resin and toughener can be adjusted by varying the molecular weight of the rubber. The best results are obtained by modifying an epoxy resin with 10 wt% of bishydroxy-terminated oligo(butylmethacrylate) of a molecular weight of 5000 g/mol. Fracture toughness K-lc increases by 150% accompanied by a decrease in modulus of only 11% and in strength of 16%, as compared to the corresponding properties of the neat resin. Due to an almost complete phase separation of the rubber upon curing, the glass transition temperature is scarcely affected. (C) 1998 John Wiley & Sons, Inc. [References: 23]
机译:基于双羟基封端的低聚(甲基丙烯酸丁酯)的新型液态橡胶用于增韧酸酐固化的环氧树脂。为了检查对重要机械性能的影响,例如韧性,强度,刚度和玻璃化转变温度,增韧剂的浓度和分子量是变化的。实验数据表明,远螯甲基丙烯酸酯是适用于环氧树脂的增韧剂。树脂和增韧剂之间的相容性可以通过改变橡胶的分子量来调节。通过用10 wt%的分子量为5000 g / mol的双羟基封端的低聚(甲基丙烯酸丁酯)改性环氧树脂可获得最佳结果。与纯树脂的相应性能相比,断裂韧性K-lc增加150%,同时模量仅降低11%,强度降低16%。由于固化时橡胶几乎完全发生相分离,因此几乎不影响玻璃化转变温度。 (C)1998 John Wiley&Sons,Inc. [参考:23]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号