Silk and wool fibers were acylated with two acid anhydrides,dodecenylsuccinic anhydride (DDSA) and octadecenylsuccinic anhydride (ODSA),at 75 deg C with N,N-dimethylformamide (DMF) or dimethyl sulfoxide (DMSO) as the solvent,the latter of which allowed higher weight gains to be reached.The weight gain and acyl content of wool was always higher than that of silk.Tensile properties of silk remained unchanged regardless of weight gain,whereas wool displayed a noticeably higher extensibility at high weight gain.Fine structural changes of acylated wool were de-tected by DSC analysis.Moisture regain and water retention of acylated silk and wool decreased significantly,whereas water repellency increased.SEM analysis showed the presence of foreign material firmly adherent to the surface of both silk and wool,whose amount increased with increasing weight gain.These deposits were attributed to the presence of the modifying agens at the fiber surface on the basis of the characteristic IR bands.The possible application of silk and wool fibers acylated with DDSA or ODSA for the preparation of water-repellent textile materials is discussed.
机译:丝绸和羊毛纤维在75摄氏度下,以N,N-二甲基甲酰胺(DMF)或二甲基亚砜(DMSO)为溶剂,用两种酸酐将十二烯基琥珀酸酐(DDSA)和十八烯基琥珀酸酐(ODSA)酰化。羊毛的重量增加和酰基含量始终比丝绸高。无论重量增加,丝绸的拉伸性能都保持不变,而羊毛在高重量增加时表现出明显更高的延展性。精细的结构变化用DSC分析法检测酰化羊毛的数量。酰化丝和羊毛的回潮率和保水率显着降低,而疏水性提高。SEM分析表明,存在异物牢固附着在丝和羊毛表面,其数量这些沉积物归因于基于特征IR谱带的纤维表面上的修饰原子的存在。讨论了用DDSA或ODSA酰化的丝和羊毛纤维在制备疏水纺织材料中的可能应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号