This paper is focused on the iron removal from sulphuric acid-zinc liquors obtained from double leached Waelz oxide. The initial iron concentration in the liquor was around 80 mg/L which must be removed prior to complementary purification stages and zinc electrowinning. Different oxidation agents were studied, operating at room temperature and atmospheric pressure. It was observed that the most suitable oxidation agent was a mixture of Mn02-H_2O_2. During 20 min at pH 4.5 while adding 2 mL H_2O_2 and 1.2 g MnO_2/L of liquor, an iron removal around 99.6% was achieved, reducing the iron concentration in the liquor to 0.3 mg/L. The proposed process operates well at room temperature and energy saving is achieved with respect to conventional oxidation processes using O_2 or H_2O_2 as oxidation agents, in which temperatures of at least 60-80 °C must be used.
机译:本文着重于从双重浸出的Waelz氧化物获得的硫酸-锌液中的铁去除。液体中的初始铁浓度约为80 mg / L,必须在补充纯化步骤和锌电解沉积之前除去。研究了在室温和大气压下运行的不同氧化剂。观察到最合适的氧化剂是MnO 2 -H_2O_2的混合物。在pH值为4.5的20分钟内,同时添加2 mL H_2O_2和1.2 g MnO_2 / L液体,除铁率约为99.6%,从而将溶液中的铁浓度降低至0.3 mg / L。所提出的方法在室温下运行良好,并且相对于使用O_2或H_2O_2作为氧化剂的常规氧化方法,可以实现节能,其中必须使用至少60-80°C的温度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号