The elevated temperature erosion behavior of three iron-base coatings sprayed by high velocity continuous combustion (HVCC) process was determined in a laboratory elevated temperature erosion tester and compared with the behavior of coatings sprayed using combustion arc-spray and standard arc-spray processes. Test conditions attempted to simulate erosion conditions found at the heat exchanger tubes in the coal-fired boilers. Two bed ashes A (highly erosive) and B (medium erosive bed ash) retrieved from two operating boilers were used as erodent materials. In addition, some other properties, such as microhardness, porosity, and oxidation rate, of coatings were also measured and compared. Erosion test results indicated that the three iron-base coatings sprayed with HVCC process demonstrated higher erosion resistance than the ones sprayed with the other two are-spray processes, when eroded by bed ash B. When eroded by high erosive ash (bed ash A), the three are-sprayed iron-base coatings exhibited similar levels of erosion resistance, the ones sprayed with HVCC process being slightly better than those sprayed with the other two processes. The difference of erosion behavior between sprayed coatings produced by different processes closely correlated with their microstructure and the characteristics of ash materials rather than the microhardness of coatings. The erosion mechanism of coatings was also discussed and compared. (C) 2001 Elsevier Science B.V. All rights reserved. [References: 13]
机译:在实验室高温腐蚀测试仪中测定了通过高速连续燃烧(HVCC)工艺喷涂的三种铁基涂层的高温腐蚀行为,并将其与使用燃烧电弧喷涂和标准电弧喷涂工艺喷涂的涂层行为进行了比较。测试条件试图模拟燃煤锅炉换热管中的腐蚀条件。从两个运行的锅炉中回收的两个灰烬A(高侵蚀性灰烬)和B(中度侵蚀性灰烬)用作侵蚀性材料。另外,还测量并比较了涂层的一些其他性能,例如显微硬度,孔隙率和氧化速率。冲蚀测试结果表明,当被床灰B侵蚀时,用HVCC工艺喷涂的三种铁基涂料显示出比其他两种正喷工艺更高的耐蚀性。 ,这三种喷涂的铁基涂料表现出相似的耐蚀性水平,用HVCC喷涂的涂料要比其他两种喷涂的涂料略好。不同工艺生产的喷涂涂层之间的腐蚀行为差异与它们的微观结构和灰分材料的特性密切相关,而不与涂层的显微硬度密切相关。还讨论并比较了涂层的腐蚀机理。 (C)2001 Elsevier Science B.V.保留所有权利。 [参考:13]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号