New thickening agents based on tamarind seed gum and karaya gum polysaccharides

机译:以罗望子种子胶和卡拉叶胶多糖为基础的新型增稠剂

获取原文
获取原文并翻译 | 示例

摘要

Wool, silk and nylon-6 fabric samples were printed with reactive dyes using new thickening agents based on polymerisation adducts of acrylic acid (AA) with tamarind seed gum (TG), or karaya gum (KG) in comparison with the conventional guar gum (GG) thickener. The obtained data indicate that: (i) the printing efficiency is governed by the performance of the thickening agents, i.e. PAA/TG2>PAA/TG1>PAA/KG1>PAA/KG2>GG, as well as the nature of substrate, i.e. wool>nylon-6 > silk, (ii) the K/S values and fastness properties of the printed fabrics are determined by the type of reactive dye, and (iii) optimal printing properties, i.e. higher depth along with better fastness ratings, were achieved by using a printing paste containing PAA/TG2 (7.5%, w/w); reactive dye (30g/kg); urea (50g/kg); and citric acid (10g/kg), followed by drying at 85 °C for 5 min, and steaming at 105 °C for 30min.
机译:羊毛,丝绸和尼龙6织物样品使用新型增稠剂用活性染料进行印花,该增稠剂基于丙烯酸(AA)与罗望子种子胶(TG)或karaya胶(KG)的聚合加合物,与传统的瓜尔豆胶( GG)增稠剂。获得的数据表明:(i)印刷效率取决于增稠剂的性能,即PAA / TG2> PAA / TG1> PAA / KG1> PAA / KG2> GG,以及底物的性质,即羊毛>尼龙-6>真丝,(ii)印花织物的K / S值和坚牢度取决于活性染料的类型,并且(iii)最佳印花性能,即更高的深度和更好的坚牢度等级通过使用含有PAA / TG2(7.5%,w / w)的印刷浆料实现;活性染料(30g / kg);尿素(50g / kg);柠檬酸(10g / kg),然后在85°C干燥5分钟,然后在105°C蒸30分钟。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号