STATEMENT OF PROBLEM: There is considerable variation in generic formulation and in reported fluoride release from resin-modified glass ionomer luting cements. PURPOSE: This study compared fluoride release from 2 generically similar resin-modified glass ionomer luting cements (Vitremer and Advance) with release from 2 conventional glass ionomer luting cements (Ketac-Cem and Fuji I). MATERIAL AND METHODS: Ten specimen disks of each of the 4 luting cements were fabricated and immersed in deionized water in individual polystyrene jars. The jars were stored in a humidor at 37 degrees C between test periods. At the same time each day, for 28 days, fluoride release from each specimen disk was measured in parts per million by testing the storage water. RESULTS: The 4 luting cements tested showed an initial high concentration of fluoride release during the first week, followed by a gradual decrease over the study period. Vitremer luting cement demonstrated the greatest mean cumulative fluoride release in parts per million over the study period (198), followed by Fuji I (140), Ketac-Cem (110), and Advance (99) luting cements. CONCLUSIONS: Resin-modified glass ionomer luting cements showed fluoride release comparable to the conventional glass ionomer luting cements. Vitremer luting cement released more fluoride over the 28-day period than the other cements.
机译:问题陈述:通用配方和树脂改性的玻璃离聚物型胶结水泥中的氟化物释放量存在很大差异。目的:本研究比较了两种通用相似的树脂改性玻璃离聚物胶结水泥(Vitremer和Advance)与两种常规玻璃离聚物胶结水泥(Ketac-Cem和Fuji I)的氟化物释放。材料与方法:制作了四种胶结水泥中的每一种的十个样品盘,并将其浸入去离子水中的各个聚苯乙烯罐中。在测试期间之间,将广口瓶存储在37摄氏度的雪茄箱中。在每天的同一时间(共28天),通过测试储存水,测量了从每个样品盘释放的氟化物(以百万分之几为单位)。结果:测试的4种胶结水泥在最初的一周内显示出最初的高浓度氟化物释放,然后在研究期间逐渐减少。在研究期间,Vitremer胶凝水泥的平均累积氟化物释放量最大,为百万分之几(198),其次是Fuji I(140),Ketac-Cem(110)和Advance(99)胶凝水泥。结论:树脂改性的玻璃离聚物胶结水泥显示出与常规玻璃离聚物胶结水泥相当的氟化物释放。 Vitremer胶泥在28天内释放的氟化物比其他水泥要多。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号