Effect of metal selection and porcelain firing on the marginal accuracy of titanium-based metal ceramic restorations.

机译:金属选择和烤瓷对钛基金属陶瓷修复体边缘精度的影响。

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

STATEMENT OF PROBLEM: Titanium is the most biocompatible metal used for dental casting; however, there is concern about its marginal accuracy after porcelain application since this aspect has direct influence on marginal fit. PURPOSE: The purpose of this study was to determine the effect that metal selection and the porcelain firing procedure have on the marginal accuracy of metal ceramic prostheses. MATERIAL AND METHODS: Cast CP Ti, milled CP Ti, cast Ti-6Al-7Nb, and cast Ni-Cr copings (n=5) were fired with compatible porcelains (Triceram for titanium-based metals and VITA VMK 95 for Ni-Cr alloy). The Ni-Cr alloy fired with its porcelain served as the control. Photographs of metal copings placed on a master die were made. Marginal discrepancy was determined on the photographs using an image processing program at 8 predetermined locations before airborne-particle abrasion for porcelain application, after firing of the opaque layer, and after firing of the dentin layer. Repeated-measures 2-way ANOVA was used to investigate the effect of metal selection and firing stage, and paired t tests were used to determine the effect of each firing stage within each material group (alpha=.05). RESULTS: ANOVA showed that both metal selection and firing stage significantly influenced the measured marginal discrepancy (P<.001), and there was interaction between the 2 variables (P<.001). Student-Newman-Keuls multiple comparison tests showed that there were significant differences between any 2 metals compared, at each stage of measurement. Paired t tests showed that significant changes in marginal discrepancy occurred with opaque firing on milled CP Ti (P=.017) and cast Ti-6Al-7Nb alloy (P=.003). CONCLUSIONS: Titanium copings fabricated by CAD/CAM demonstrated the least marginal discrepancy among all groups, while the base metal (Ni-Cr) groups exhibited the most discrepancy of all groups tested.
机译:问题陈述:钛是用于牙科铸造的生物相容性最高的金属。然而,由于其在边缘贴合性上有直接影响,因此在瓷器使用后其边缘精度会受到关注。目的:本研究的目的是确定金属选择和烤瓷程序对金属陶瓷假体的边缘精度的影响。材料和方法:用兼容的瓷器(三氟甲烷用于钛基金属和VITA VMK 95用于镍铬合金)烧制铸造CP Ti,碾磨CP Ti,铸造Ti-6Al-7Nb和铸造Ni-Cr涂层(n = 5)。合金)。以瓷器烧制的镍铬合金为对照。制作了放置在母模上的金属帽的照片。使用图像处理程序在照片上的边缘上的差异是在8个预定位置上进行的,以确定在瓷器应用的气载颗粒磨损之前,烧结不透明层之后以及烧结牙本质层之后的8个预定位置。重复测量2次方差分析用于研究金属选择和烧成阶段的影响,配对t检验用于确定每个材料组中每个烧成阶段的影响(alpha = .05)。结果:方差分析表明金属选择和烧成阶段均显着影响测得的边际差异(P <.001),并且两个变量之间存在相互作用(P <.001)。 Student-Newman-Keuls多重比较测试表明,在每个测量阶段,所比较的任何两种金属之间都存在显着差异。配对的t检验表明,在铣削的CP Ti(P = .017)和铸造的Ti-6Al-7Nb合金(P = .003)上进行不透明烧成时,边际差异发生了显着变化。结论:由CAD / CAM制造的钛合金顶盖在所有组中显示出最小的边缘差异,而贱金属(Ni-Cr)组在所有测试组中表现出最大的差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号