Wear comparison between conventional and highly cross-linked polyethylene against a zirconia head: A concise follow-up, at an average 10 years, of a previous report

机译:常规和高度交联的聚乙烯与氧化锆头的磨损比较:对先前报告的平均10年的简要随访

获取原文
获取原文并翻译 | 示例
       

摘要

We previously reported the results of wear comparison at a minimum of 5. years between highly cross-linked polyethylene (HXLPE) and conventional polyethylene (PE) against a zirconia femoral head. We now report the mean wear at 10. years for 52 patients (56 hips) of the original cohort of 61 patients (65 hips) who had undergone primary total hip arthroplasty at our hospital between November 1999 and August 2000. The mean steady-state linear wear rate of HXLPE was 0.045. mm/y, compared with 0.080. mm/y for conventional PE (P= .0003). The incidence of osteolysis was 25% in the conventional PE group compared with 0% in the HXLPE group. Our study demonstrated that the steady-state wear rate for HXLPE remains significantly lower than that for conventional PE against a zirconia femoral head at a mean of 10. years after implantation.
机译:我们之前曾报道过高度交联的聚乙烯(HXLPE)和常规的聚乙烯(PE)在氧化锆股骨头上的磨损比较结果至少为5年。现在,我们报告在1999年11月至2000年8月间在我院进行了一次原发性全髋关节置换术的61例患者(65髋)的原始队列中的52例患者(56髋)的10年平均磨损。平均稳态HXLPE的线性磨损率为0.045。毫米/年,而0.080。常规PE的mm / y(P = .0003)。常规PE组的骨溶解发生率为25%,而HXLPE组为0%。我们的研究表明,植入后平均10年,HXLPE的稳态磨损率仍然显着低于传统PE对氧化锆股骨头的磨损率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号