首页> 外文期刊>The Journal of arthroplasty >Wear comparison between a highly cross-linked polyethylene and conventional polyethylene against a zirconia femoral head: minimum 5-year follow-up.
【24h】

Wear comparison between a highly cross-linked polyethylene and conventional polyethylene against a zirconia femoral head: minimum 5-year follow-up.

机译:高度交联的聚乙烯和常规聚乙烯与氧化锆股骨头之间的磨损比较:至少5年随访。

获取原文
获取原文并翻译 | 示例
       

摘要

Highly cross-linked polyethylene (HXLPE) was developed to reduce wear of articular bearing surface in total hip arthroplasty patients. Several studies have shown reduced wear of HXLPE compared with conventional polyethylene; however, these studies had used HXLPE in combination with a Co-Cr metal head. The purpose of this study was to compare the 5-year in vivo wear of HXLPE with that of conventional PE using a zirconia femoral head. Forty-five hips with a Trilogy HXLPE (Zimmer, Warsaw, Ind) were matched and compared with a control group of 20 conventional Trilogy PE hips. The 2-dimensional linear wear rate was significantly less in the HXLPE group between 1 and 5 years postoperation (P < .001). The results show that HXLPE reduces short-term polyethylene wear against not only a Co-Cr head but also a zirconia head.
机译:开发了高度交联的聚乙烯(HXLPE),以减少全髋关节置换患者的关节轴承表面的磨损。多项研究表明,与传统的聚乙烯相比,HXLPE的磨损有所减少;然而,这些研究将HXLPE与Co-Cr金属头结合使用。这项研究的目的是比较HXLPE与使用氧化锆股骨头的传统PE在体内的5年佩戴情况。匹配三支带有Trilogy HXLPE(Zimmer,华沙,印第安纳州)的髋关节,并将其与20个常规Trilogy PE髋关节的对照组进行比较。 HXLPE组术后1至5年间的二维线性磨损率显着降低(P <.001)。结果表明,HXLPE不仅可以降低聚乙烯短期对Co-Cr头的磨损,而且还可以降低氧化锆头的磨损。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号