首页> 外文期刊>Quintessence international >Antibacterial activity and tensile strength of provisional cements modified with fluoridecontaining varnish.
【24h】

Antibacterial activity and tensile strength of provisional cements modified with fluoridecontaining varnish.

机译:含氟清漆改性的临时水泥的抗菌活性和抗张强度。

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Objective: To test three noneugenol provisional cements (TempBond NE, RelyX Temp NE, and Freegenol) for their antibacterial properties and to test the hypothesis that addition of fluoride varnish confers antibacterial properties on these provisional cements without compromising their tensile strength. Method and Materials: A total of 576 cylindrical samples were prepared (96 of each of six types) from three noneugenol provisional cements, both unmodified and modified by the addition of 5% w/w Duraphat fluoride varnish. The samples were aged in saline that was replaced twice a week for up to 90 days. Twenty-four samples of each type were removed from the saline at 1, 7, 30, or 90 days and assessed for antibacterial properties against Streptococcus mutans by using an agar diffusion test (n = 12) and tensile strength by using a diametral tensile strength test (n = 12). Data were subjected to one- and three-way ANOVA, the Tukey honestly significant difference test, and t test at a significance level of .002 (P < .002). Results: TempBond NE had no antibacterial activity in its unmodified form but showed antibacterial activity when modified by the addition of 5% w/w fluoride varnish. Freegenol had the highest antibacterial activity in its unmodified form, which was not altered by the addition of the varnish. RelyX Temp NE had mild antibacterial activity that was slightly enhanced by adding the varnish. Adding the varnish reduced the tensile strength of TempBond NE and Freegenol, but did not affect the tensile strength of RelyX Temp NE. Conclusion: Antibacterial activity was observed for the unmodified form of Freegenol and TempBond NE after the addition of the fluoride varnish. The addition of the fluoride varnish reduced the tensile strength of both TempBond NE and Freegenol.
机译:目的:测试三种非丁香酚临时水泥(TempBond NE,RelyX Temp NE和Freegenol)的抗菌性能,并测试以下假设:添加氟化物清漆可赋予这些临时水泥抗菌性能而不会损害其抗张强度。方法和材料:用三种非丁香酚临时胶合剂共制备了576个圆柱形样品(六种类型中的每种96种),未改性和通过添加5%w / w Duraphat氟化清漆改性。样品在盐水中老化,每周更换两次,最多90天。在第1、7、30或90天从盐水中取出每种类型的二十四个样品,并通过琼脂扩散试验(n = 12)评估其对变形链球菌的抗菌性能,并使用直径拉伸强度评估其拉伸强度测试(n = 12)。数据接受了单向和三向方差分析,Tukey诚实的显着差异检验和t检验,显着性水平为0.002(P <.002)。结果:TempBond NE的未修饰形式没有抗菌活性,但是通过添加5%w / w氟化清漆进行修饰后却显示出抗菌活性。 Freegenol的未修饰形式具有最高的抗菌活性,添加清漆不会改变它的活性。 RelyX Temp NE具有适度的抗菌活性,添加清漆后其活性略有增强。添加清漆会降低TempBond NE和Freegenol的拉伸强度,但不会影响RelyX Temp NE的拉伸强度。结论:添加氟化清漆后,未改性形式的Freegenol和TempBond NE具有抗菌活性。氟化物清漆的加入降低了TempBond NE和Freegenol的拉伸强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号