The effect of electromagnetic stirring and cerium addition on dry sliding reciprocating wear of hypereutectic aluminium-silicon alloy

机译:电磁搅拌和铈添加对过共晶铝硅合金干式往复往复磨损的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Influences of electromagnetic stirring (EMS) and rare earth (RE) CeO_2 addition on reciprocating wear behaviour of hypereutectic Al-Si alloys have been presented in this article. Reciprocating wear tests were carried out at different contact loads (from 15 to 90 N) and speeds (from 0.2 to 1.0 m/s) using pin-on-plate configuration for a constant sliding distance of 500 m. It was observed that EMS and RE (CeO_2) addition refined the microstructure and improved the hardness. EMS reduced the wear rates of hypereutectic Al-Si alloy irrespective of applied load and sliding velocity. Transition from mild to severe wear was observed in as-cast alloy at 90 N normal load (constant sliding velocity = 0.4 m/s). Scanning electron microscopy of worn surfaces and wear debris was carried out to study the wear mechanism of material removal under different sliding conditions.
机译:本文介绍了电磁搅拌(EMS)和稀土(RE)CeO_2添加对过共晶Al-Si合金往复磨损行为的影响。使用销上板配置在500 m的恒定滑动距离下,在不同的接触负载(15至90 N)和速度(0.2至1.0 m / s)下进行往复磨损测试。观察到,添加EMS和RE(CeO_2)可以改善微观结构并提高硬度。 EMS降低了过共晶Al-Si合金的磨损率,而与施加的载荷和滑动速度无关。在90 N的正常载荷下(恒定滑动速度= 0.4 m / s),在铸态合金中观察到了从轻度磨损到严重磨损的转变。进行了磨损表面和磨损碎片的扫描电子显微镜研究,以研究在不同滑动条件下材料去除的磨损机理。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号