Simultaneous absorption of SO2 and NO_x with pyrolusite slurry combined with gas-phase oxidation of NO using ozone: Effect of molar ratio of O2/(SO2 + 0.5NO_x) in flue gas

机译:软锰矿浆同时吸收SO2和NO_x并利用臭氧进行NO气相氧化:烟气中O2 /(SO2 + 0.5NO_x)摩尔比的影响

获取原文
获取原文并翻译 | 示例
       

摘要

NO in flue gas was oxidized into NO2 by ozone in gas-phase first, and then SO2 and NO2 were oxidized by redox reaction between MnO2 and SO2/NO2 and catalyzed oxidation between 02 and SO2/NO2 in absorption process. Molar ratio of O2/(SO2 + 0.5NO_x) in flue gas had a decisive effect on catalyzed oxidation in absorption process, and eventually influenced reaction byproducts, Mn extraction rate and SO2/NO_x absorption capability. Results showed that increasing O2/(SO2 + 0.5NO_x) enhanced catalyzed oxidation and led to the lower reaction pH. When O2/(SO2 + 0.5NO_x) ≤ 18, SO2 and NO_x were mainly oxidized by MnO2 with main products of MnSO4 and Mn(NO3)2, while when O2/(SO2 + 0.5NO_x) ≥ 18, SO2 and NO_x were mainly oxidized by O2 with main products of H2SO4 arid HNO3. Total absorption capability of SO2 and NO, increased with increasing O2/(SO2 + 0.5NO_x). Mn extraction rate increased with the increase of O2/(SO2 + 0.5NO_x) first and then decreased, the maximum Mn extraction rate of 91% was got when O2/ (SO2 + 0.5NO_x) at around 13. Both the SO2/NO_x absorption capability and Mn extraction rate could be enhanced by adding rhodochrosite as pH regulator in the case of O2/(SO2 + 0.5NO_x) ≥ 18.
机译:烟气中的NO首先被气相中的臭氧氧化为NO2,然后通过MnO2与SO2 / NO2之间的氧化还原反应氧化SO2和NO2,并在吸收过程中催化02与SO2 / NO2之间的氧化。烟气中O2 /(SO2 + 0.5NO_x)的摩尔比对吸收过程中的催化氧化起决定性作用,最终影响反应副产物,锰的萃取率和SO2 / NO_x的吸收能力。结果表明,增加O2 /(SO2 + 0.5NO_x)可以增强催化氧化作用,并导致较低的反应pH。当O2 /(SO2 + 0.5NO_x)≤18时,MnO2会以MnSO4和Mn(NO3)2的主要产物氧化SO2和NO_x,而当O2 /(SO2 + 0.5NO_x)≥18时,SO2和NO_x则主要被MnO2氧化。被H2SO4和HNO3的主要产物O2氧化。 SO2和NO的总吸收能力随O2 /(SO2 + 0.5NO_x)的增加而增加。 Mn的提取率先随O2 /(SO2 + 0.5NO_x)的增加而增加,然后降低,当O2 /(SO2 + 0.5NO_x)在13左右时,锰的最大提取率达到91%。在O2 /(SO2 + 0.5NO_x)≥18的情况下,加入菱锰矿作为pH调节剂,可提高其能力和Mn的萃取率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号