Comparison of Superpave and Marshall Mix Performance in Alabama

机译:Superpave和Marshall混合料在阿拉巴马州的性能比较

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The Alabama Department of Transportation specifies the Superpave~® design system for most of its dense-graded HMA mixes. However, there is concern that the number of design gyrations (N_(Design)) may be too high for specified traffic levels. Mixes designed with an N_(Design) level that is too high would be rut resistant but may be difficult to compact in the field and may suffer from durability problems such as premature cracking and raveling. The objective of this project is to evaluate the performance of Alabama's mixes designed according to Superpave criteria and compare them to the performance of Alabama's Marshall-designed mixes to determine whether current N_(Design) levels should be adjusted. The following conclusions are based on an evaluation of 25 Marshall and Superpave projects placed about the same time and serving under approximately the same traffic conditions: (a) Generally, both Marshall and Superpave mixtures are performing quite well with little rutting and cracking after a period of about 4 years. (b) It is likely that most Marshall and Superpave mixtures will not reach the design air voids of 4.0% during the life of the pavement. After 4 years, the average air voids measured in the wheelpaths was 5.3% for Marshall mixes and 5.9% for Superpave mixtures. (c) It appears that the durability of Superpave mixtures can be improved, without adversely affecting the rutting resistance, by increasing the asphalt content. Practitioners, however, are cautioned to monitor rutting indicators closely during mixture design, production, and construction.
机译:阿拉巴马州交通运输部为其大部分致密等级的HMA混合物指定了Superpave〜®设计系统。但是,对于指定的通信量水平,设计回转数(N_(Design))可能会过高。 N_(设计)水平过高的混合物将具有耐车辙性,但在现场可能难以压实,并且可能会遇到耐久性问题,例如过早开裂和开裂。该项目的目的是评估根据Superpave标准设计的阿拉巴马州混合物的性能,并将其与阿拉巴马州马歇尔设计的混合物的性能进行比较,以确定是否应调整当前的N_(Design)水平。以下结论基于对25个大约同时放置并在相同交通条件下服务的Marshall和Superpave项目的评估:(a)通常,Marshall和Superpave混合物的性能都很好,经过一段时间后几乎没有车辙和开裂大约4年。 (b)大多数Marshall和Superpave混合物在路面寿命期间可能不会达到4.0%的设计气隙。 4年后,在轮径中测得的平均气隙对于Marshall混合物为5.3%,对于Superpave混合物为5.9%。 (c)通过增加沥青含量,可以改善Superpave混合物的耐久性,而不会不利地影响耐车辙性。但是,从业人员应注意在混合物设计,生产和施工期间密切监控车辙指标。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号