In this work, lanthanum oxide (La2O3) has been studied for the methane partial oxidation reaction. We report long term experimental studies on La2O3, prepared by the solution combustion method with 5 wt% of Ni being added using chemical reduction method. Thorough characterization is done using XRD, SEM and FTIR. The activity is measured in terms of methane conversion and hydrogen and carbon monoxide selectivity. Methane oxidation is also carried out by varying the residence time, which changes the product distribution. Furthermore, methane activity is studied in the absence of oxygen and effect of pretreatment is also disused in detail. It is observed that the addition of nickel on the La2O3 catalyst (5 % Ni/La2O3) increases the catalytic activity significantly. Long term tests at isothermal conditions on both La2O3 and 5 % Ni/La2O3 catalysts are carried out to study the deteriorating effect of carbon (coke) deposition. Hydrogen production with 5 % Ni/La2O3 is significantly enhanced compared to La2O3, and it is experimentally observed that both the catalysts show excellent coking resistance capabilities.
机译:在这项工作中,已经研究了氧化镧(La2O3)用于甲烷部分氧化反应。我们报告了通过固溶燃烧方法制备的La2O3的长期实验研究,其中使用化学还原方法添加了5 wt%的Ni。使用XRD,SEM和FTIR进行了彻底的表征。根据甲烷转化率以及氢和一氧化碳的选择性来测量活性。甲烷氧化还可以通过改变停留时间来进行,这会改变产物的分布。此外,在没有氧气的情况下研究了甲烷的活性,并且也没有详细说明预处理的作用。可以看出,在La2O3催化剂上添加镍(5%Ni / La2O3)可显着提高催化活性。对La2O3和5%Ni / La2O3催化剂在等温条件下进行了长期测试,以研究碳(焦炭)沉积的恶化作用。与La2O3相比,Ni / La2O3含量为5%的氢气的产生显着增强,并且实验观察到两种催化剂均显示出优异的抗结焦能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号