Effect of compatibiliser on the biodegradation and mechanical properties of high-content starch/low-density polyethylene blends

机译:相容剂对高含量淀粉/低密度聚乙烯共混物生物降解和力学性能的影响

获取原文
获取原文并翻译 | 示例

摘要

A high-content starch/low-density polyethylene (LDPE) blend with acceptable biodegradation and mechanical properties was produced by adjusting the compatibility of the blend system and processing plasticisation through the compatibiliser and different processing method. Two kinds of compatibilisers, maleic anhydride grafted LDPE after plasma treatment (MA-g-PLDPE) and acrylic acid grafted LDPE after plasma treatment (AAc-g-PLDPE), were synthesized and used in this work. The grafting degree (GD) of MA-g-PLDPE was 1.90 X 10~(-4) mol/g. The GD of AAc-g-PLDPE was 2.5 X 10~(-4) mol/g. MA-g-PLDPE gave more compatibility than AAc-g-PLDPE by the anhydride groups. The plasticisation effect by the oligomer resulted from a different process by mixing the MA-g-PLDPE and/or maleic anhydride (MA) with glycerol before compounding was investigated. As the MA and compatibiliser/LDPE premixed with GA for 30 min, the LDPE particle size of blends decreased with increasing compatibiliser content. If the free MA was not added, the PE blends show irregular shapes. The weight loss of all samples achieved above 65 wt% after two weeks of biodegradation. The weight losses of blends that contain free MA were higher than those without free MA. Finally, the structure of blends after soil burial was observed by SEM.
机译:通过调节共混体系的相容性并通过增容剂和不同的加工方法加工增塑剂,可以生产出具有良好生物降解性和机械性能的高含量淀粉/低密度聚乙烯(LDPE)共混物。合成了两种相容剂,等离子处理后的马来酸酐接枝LDPE(MA-g-PLDPE)和等离子处理后的丙烯酸接枝的LDPE(AAc-g-PLDPE)。 MA-g-PLDPE的接枝度(GD)为1.90 X 10〜(-4)mol / g。 AAc-g-PLDPE的GD为2.5 X 10〜(-4)mol / g。通过酸酐基团,MA-g-PLDPE比AAc-g-PLDPE具有更大的相容性。在配混之前,通过将MA-g-PLDPE和/或马来酸酐(MA)与甘油混合,可以通过不同的方法获得低聚物的增塑效果。随着MA和相容剂/ LDPE与GA预混合30分钟,混合物的LDPE粒径随着相容剂含量的增加而减小。如果未添加游离MA,则PE共混物显示不规则形状。经过两周的生物降解,所有样品的重量损失均达到了65 wt%以上。含有游离MA的共混物的重量损失高于不含游离MA的那些。最后,用SEM观察了土埋后的掺混物结构。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号