首页> 外文期刊>日本金属学会誌 >Mg-Ca二元系亜共晶合金における高温クリープ挙動
【24h】

Mg-Ca二元系亜共晶合金における高温クリープ挙動

机译:Mg-Ca二元次共晶合金的高温蠕变行为

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

The creep behavior of hypoeutectic Mg_(1-x)Ca_x(x = 2.8, 8.7, and 14.8mass%) cast alloys was investigated at 473 K under stresses between 30 and 60 MPa. The microstructure of the alloys is characterized by the discontinuously distributed primary α-Mg phase in a continuous eutectic fine lamellar structure consisting of α-Mg and C14-Mg_2Ca phases. The creep curves of the alloys exhibit three stages: a normal transient creep stage, a minimum creep rate stage and finally an accelerating stage. The decrease in creep rate during the transient stage becomes pronounced and the onset of the accelerating stage is delayed with increasing calcium concentration. The stress exponent of the minimum creep rate is four for each alloy for stresses below the yield stress. The creep of the alloys is controlled by the high-temperature climb of dislocations. The effect of the eutectic fine lamellar structure on creep strength is prominent when the volume fraction is below 50%.%マグネシウム合金は,自動車の高燃費を達成し二酸化炭素排出量を最小化するために,自動車用軽量構造材料として興味を持たれている.現在,マグネシウム合金の適用は,エンジンブロックやエンジンクレードルへの極めて限られた使用例を除いて,室温部材に限定されている.
机译:研究了亚共晶Mg_(1-x)Ca_x(x = 2.8、8.7和14.8mass%)铸造合金在473 K下在30至60 MPa应力下的蠕变行为。合金的显微组织的特征在于,在由α-Mg和C14-Mg_2Ca相组成的连续共晶细薄层状结构中,不连续分布的初生α-Mg相。合金的蠕变曲线表现出三个阶段:正常的瞬态蠕变阶段,最小蠕变速率阶段以及最后的加速阶段。在过渡阶段蠕变速率的降低变得明显,并且随着钙浓度的增加,加速阶段的开始被延迟。对于低于屈服应力的应力,每种合金的最小蠕变速率的应力指数为4。合金的蠕变受位错的高温爬升控制。当体积分数低于50%时,共晶细小层状结构对蠕变强度的影响就很明显。%マグネシウム现在,マグネシウム合金の适用は,エンジンブロックやエンジンクレードルへの极めて限られた使用例を除いて,室内部材に限定されている。

著录项

  • 来源
    《日本金属学会誌》 |2012年第4期|p.251-255|共5页
  • 作者单位

    名古屋大学大学院工学研究科マテリアル理工学専攻;

    名古屋大学大学院工学研究科マテリアル理工学専攻,東京工業大学;

    名古屋大学大学院工学研究科マテリアル理工学専攻;

    名古屋大学大学院工学研究科マテリアル理工学専攻;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 jpn
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号