A two-step thermal process, an initial thermal treatment at mild temperature followed by a fast pyrolysis step, was investigated to recover wood preservatives and produce preservatives-free wood for production of high quality bio-oil from used creosote-treated railroad ties. During the initial thermal treatment at temperature of 280 degrees C for 10-30 min, the treated wood ties underwent a 20-25% weight loss with energy yield (77-83%). Energy yield at 280 degrees C was lower than that at 200 and 250 degrees C (92-97%) but higher than that at the 300 degrees C (64-74%). Recovery level of creosote at 280 degrees C was comparable to that at 300 degrees C. Fast pyrolysis at 450 degrees C of the 280 degrees C-treated wood ties produced high amount of levoglucosan and phenolic compounds with a traceable amount (1.7-1.9% of the total peak area) of creosote compounds. (C) 2015 Elsevier Ltd. All rights reserved.
机译:研究了两个步骤的热过程,即在温和的温度下进行初始热处理,然后进行快速热解步骤,以回收木材防腐剂并生产不含防腐剂的木材,以便从用过的经过杂酚油处理的铁路枕木生产高质量的生物油。在280摄氏度的温度下进行10-30分钟的初始热处理期间,经过处理的木扎带重量减少了20-25%,能量产生率(77-83%)。 280℃下的能量产率低于200℃和250℃下的能量产率(92-97%),但高于300℃下的能量产率(64-74%)。杂酚油在280摄氏度下的回收水平与300摄氏度下的相当。在280摄氏度处理的木扎带在450摄氏度下快速热解产生大量左旋葡聚糖和酚类化合物,含量可追溯(1.7-1.9%杂酚化合物的总峰面积)。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号