Dielectric behavior of insulating materials under liquid nitrogen

机译:液氮下绝缘材料的介电行为

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Measurements were made to assess the AC breakdown voltages in liquid nitrogen (LN/sub 2/) with different electrode configurations such as sphere-sphere, needle-needle, hemisphere-hemisphere, plane-plane, sphere-needle, etc. Experimental results reveal that the breakdown voltage is a function of electrode geometry and gap length. This study also addresses the effect on the breakdown strength of solid insulating materials under LN/sub 2/ environment with a sphere-sphere electrode configuration. In this paper, special emphasis has been attributed to the effect on loss index of a variety of dielectrics dipped in LN/sub 2/. The measured values of breakdown strength and loss index have been compared with those obtained under atmospheric condition. The study reveals that the breakdown strength of cellulosic materials like paper or pressboard increases manifold while the loss index decreases significantly when dipped in LN/sub 2/ with variations of the order of 50% to 90%. However, for impervious noncellulosic materials like Perspex (acrylic glass) or presspahn, the increase in breakdown strength is not that pronounced and the decrease in loss index is of the order of 2 to 30%.
机译:进行了测量以评估具有不同电极配置(例如球形,球形,针形,半球形,半球形,平面形,球形针形等)的液氮中的AC击穿电压(LN / sub 2 /)。实验结果表明击穿电压是电极几何形状和间隙长度的函数。这项研究还解决了在球形电极结构下LN / sub 2 /环境下对固体绝缘材料击穿强度的影响。本文特别强调了浸入LN / sub 2 /中的各种电介质对损耗指数的影响。将击穿强度和损耗指数的测量值与在大气条件下获得的值进行了比较。研究表明,当浸入LN / sub 2 /中时,纤维素材料(如纸或压纸板)的击穿强度会增加,而损耗指数会显着下降,变化幅度约为50%至90%。但是,对于不可渗透的非纤维素材料,如有机玻璃(丙烯酸玻璃)或压榨机,其击穿强度的提高并不明显,损耗指数的降低约为2%至30%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号