PbS thin films with thickness between 100 and 150 nm were grown for the first time by microwave-assisted chemical bath deposition in a commercial automated system with deposition times not exceeding 5 min. X-ray diffraction analysis shows that the thin films have cubic rock salt type structure with good crystallinity. The grain size increased from 18 to 20 nm, as the deposition time increased. Energy dispersive X-ray results confirm that the films are stoichiometric. Optical measurements show that thin films have relatively high absorption coefficients between 104 and 105 cm-1 in the visible range. In addition, the films exhibit a direct gap, within the energy range from 1.0 to 1.35 eV. The electrical properties, such as conductivity, the Seebeck coefficient, carrier concentration, and carrier mobility, are discussed.
机译:通过微波辅助化学浴沉积在商业自动化系统中首次生长厚度在100和150nm之间的PBS薄膜,其沉积时间不超过5分钟。 X射线衍射分析表明,薄膜具有良好结晶度的立方岩盐型结构。随着沉积时间的增加,晶粒尺寸从18至20nm增加。能量分散X射线结果证实薄膜是化学计量的。光学测量表明,薄膜在可见范围内具有104至105cm-1之间的相对高的吸收系数。此外,薄膜在1.0至1.35eV的能量范围内表现出直接间隙。讨论了电性能,例如电导率,塞贝克系数,载流子浓度和载流子迁移率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号