Sonochemical technology is a technology that involves ultrasonic waves in chemical reactions. In this study, humic acid isolated from peat soil has been successfully modified with magnetite (HA-Fe3O4) using sonochemical technology. Characterization of the physical and chemical properties of HA-Fe3O4 was carried out using FTIR, XRD, SEM and VSM. HA-Fe3O4 was used for recovery of gold from simulated gold waste (HAuCl4). FTIR characterization showed that the interaction between HA and Fe3O4 was through hydrogen bonds. The crystal size of HA-Fe3O4 using the Debye-Scherrer equation based on the XRD diffractogram was 12.4 nm. The saturation magnetization value of HA-Fe3O4 obtained was 52.80 emu/g. Adsorption studies at various pH showed that HA-Fe3O4 has been successful in recovering of gold from simulated gold waste. The % recovery of gold was 99%. Gold recovery occurs through the adsorption process followed by reduction of Au (III) to Au(0).
机译:Sonochemical技术是一种涉及化学反应中的超声波的技术。在这项研究中,使用SONOCHEMICAL技术成功地用磁铁矿(HA-FE3O4)成功修饰了从泥炭土中分离的腐殖酸。使用FTIR,XRD,SEM和VSM进行HA-Fe3O4的物理和化学性质的表征。 HA-Fe3O4用于从模拟金废物(HauCl4)中回收黄金。 FTIR表征表明,HA和Fe3O4之间的相互作用是通过氢键。使用基于XRD衍射图的Deybe-Scherrer方程的HA-Fe3O4的晶体尺寸为12.4nm。所得HA-Fe 3 O 4的饱和磁化值为52.80 emu / g。各种pH的吸附研究表明,HA-Fe3O4已成功地从模拟金废物中恢复黄金。黄金的%回收率为99%。通过吸附过程发生金回收,然后通过减少Au(iii)至au(0)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号