Multiblock copolymers consisting of poly( g-benzyl L-glutamate) (PBLG) as the hydrophobic part and poly(ethylene oxide) (PEO) as the hydrophilic part (GEG) were synthesized and characterized. GEG polymeric micelles were prepared by the dialysis technique. Particle size distributions based on intensity,volume, and number-average were 22.6 【 11.9 nm, 23.5 【 4.6 nm, and 23.7 【 37 nm, respectively. It was observed that par-ticle size and size distribution of GEG polymeric micelles changed significantly with the choice of initial sol-vent. Transmission electron micrographs (TEM) showed the polymeric micelles to be spherically shaped, with sizes ranging from 20 nm to 40 nm in diameter. Fluorescence spectroscopy measurements suggested that GEG block copolymers wereassociated in water to form polymeric micelles, and the critical micelle concentrations (CMC) value of the block copolymers was 0.0094 g/L. Further evidenceof micelle formation of GEG block copolymers and limited mobility of the PBLG chain in the core ohe micelle was obtained with 1 H NMR in D2O.
机译:合成并表征了由聚(g-苄基L-谷氨酸)(PBLG)作为疏水部分和聚(环氧乙烷)(PEO)作为亲水部分(GEG)组成的多嵌段共聚物。通过透析技术制备GEG聚合物胶束。基于强度,体积和数均的粒径分布分别为22.6【11.9nm】,23.5【4.6nm和23.7【37nm。观察到,随着初始溶剂的选择,GEG聚合物胶束的颗粒尺寸和尺寸分布发生了显着变化。透射电子显微照片(TEM)显示聚合物胶束为球形,直径范围为20nm至40nm。荧光光谱测量表明,GEG嵌段共聚物在水中缔合形成聚合物胶束,该嵌段共聚物的临界胶束浓度(CMC)值为0.0094g / L。用1 H NMR在D2O中获得了GEG嵌段共聚物的胶束形成和PBLG链在胶束核心中流动性有限的进一步证据。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号