We aimed to examine the effect of various adhesive systems on the bond strength of composite resin to enamel or dentin prepared with erbium, chromium: yttrium scandium gallium garnet (Er,Cr:YSGG) laser. Each laser-cut enamel or dentin surface was treated with a bonding agent (SBB, Group 1); self-etching primer (SBP) and SBB (Group 2 and control); phosphoric-acid (KET), SBP and SBB (Group 3); KET, sodium-hypochlorite (ADG), SBP and SBB (Group 4); all-in-one adhesive (TSB, Group 5); or KET, ADG and TSB (Group 6). The control group was only polished with wet silicon carbide papers. The enamel shear bond strength of Group 5 was significantly lower than that of other groups (p <0.01). The control group showed higher bond strength compared to Groups 1–6 (p <0.05). Preconditioning using phosphoric acid or phosphoric acid followed by sodium hypochlorite increased the bond strength of composite resin to enamel and dentin prepared using an Er,Cr:YSGG laser.
机译:我们旨在研究各种粘合剂体系对复合树脂与用to,铬:钇scan镓石榴石(Er,Cr:YSGG)激光制备的牙釉质或牙本质的粘合强度的影响。每个激光切割的瓷釉或牙本质表面均用粘合剂处理(SBB,组1);自蚀刻底漆(SBP)和SBB(第2组和对照);磷酸(KET),SBP和SBB(第3组); KET,次氯酸钠(ADG),SBP和SBB(第4组);多合一粘合剂(TSB,第5组);或KET,ADG和TSB(第6组)。对照组仅用湿的碳化硅纸抛光。第5组的牙釉质剪切粘合强度显着低于其他组(p <0.01)。与1-6组相比,对照组显示出更高的结合强度(p <0.05)。使用磷酸或磷酸再用次氯酸钠进行预处理可提高复合树脂与使用Er,Cr:YSGG激光制备的牙釉质和牙本质的结合强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号