Background Polymethyl-methacrylate (PMMA) beads releasing antibiotics are used extensively to treat osteomyelitis, but require surgical removal afterwards because they do not degrade. Methods As an alternative option, this report compares the in vitro gentamicin release profile from clinically used, biodegradable carrier-materials: six injectable cements and six granule-types. Cement cylinders and coated granules containing 3% gentamicin were submerged in dH2O and placed in a 48-sample parallel drug-release system. At regular intervals (30, 90, 180 min. and then every 24 h, for 21 days), the release fluid was exchanged and the gentamicin concentration was measured. The activity of released gentamicin was tested on Staphylococcus aureus . Results All combinations showed initial burst-release of active gentamicin, two cements had continuous-release (17 days). The relative release of all cements (36–85%) and granules (30–62%) was higher than previously reported for injectable PMMA-cements (up to 17%) and comparable to other biodegradable carriers. From the cements residual gentamicin could be extracted, whereas the granules released all gentamicin that had adhered to the surface. Conclusion The high release achieved shows great promise for clinical application of these biodegradable drug-carriers. Using the appropriate combination, the required release profile (burst or sustained) may be achieved.
机译:背景技术释放抗生素的聚甲基丙烯酸甲酯(PMMA)珠子被广泛用于治疗骨髓炎,但由于它们不会降解,因此需要手术切除。方法作为替代选择,本报告比较了临床使用的可生物降解载体材料中的庆大霉素的体外释放曲线:六种可注射的水泥和六种颗粒类型。将含有3%庆大霉素的水泥瓶和包衣颗粒浸入dH 2 O中,并放入48个样品的平行药物释放系统中。定期(30、90、180分钟,然后每24小时,共21天)更换释放液并测量庆大霉素浓度。在金黄色葡萄球菌上测定了庆大霉素的释放活性。结果所有组合均显示出活性庆大霉素的初始释放,两种胶结剂均具有连续释放(17天)。所有水泥的相对释放量(36-85%)和颗粒的相对释放量(30-62%)高于以前报道的可注射PMMA水泥(最高17%),与其他可生物降解的载体相当。可以从水泥中提取残留的庆大霉素,而颗粒释放出所有粘附在表面的庆大霉素。结论所获得的高释放量为这些可生物降解的药物载体的临床应用提供了广阔的前景。使用适当的组合,可以实现所需的释放曲线(爆发或持续)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号