首页> 外文期刊>Biofouling >The Prevention Of Microfouling And Macrofouling On Hydrogels Impregnated With Either Arquad 2c-75~r Or Benzalkonium Chloride
【24h】

The Prevention Of Microfouling And Macrofouling On Hydrogels Impregnated With Either Arquad 2c-75~r Or Benzalkonium Chloride

机译:Arquad 2c-75〜r或苯扎氯铵浸渍的水凝胶的微污垢和大污垢的预防

获取原文
获取原文并翻译 | 示例

摘要

Optically clear,surfactant loaded poly (2-hydroxyethyl methacrylate) (pHEMA) hydrogels can be used to prevent fouling on optical windows of marine underwater sensors.To act successfully in this capacity,hydrogels need to prevent both microfouling and macrofouling.Panel trials were conducted using four different materials: unloaded hydrogels,hydrogels containing either benzalkonium chloride (BAC) or dicocodimethylammonium chloride (Arquad 2C-75~R) and PMMA coupons.Three panels were deployed at staggered intervals (2,4 and 6 weeks) before the main settlement season of Semibalanus balanoides and Mytilus edulis in the Firth of Clyde,Scotland.Panels were left for a total period of 10,12 and 14 weeks respectively.Results showed that no sample completely resisted fouling,but Arquad 2C-75~R hydrogels were extremely effective at preventing both microfouling and macrofouling.The most heavily fouled materials were unloaded hydrogels and PMMA,despite differences in initial hydrophilicities.Arquad 2C-75~R hydrogels were equally effective at preventing larval settlement,for up to 14 weeks.
机译:光学透明,载有表面活性剂的聚甲基丙烯酸2-羟乙酯(pHEMA)水凝胶可用于防止船用水下传感器的光学窗上结垢。为成功发挥这种作用,水凝胶需要同时防止微结垢和大结垢。使用四种不同的材料:空载水凝胶,包含苯扎氯铵(BAC)或二可可二甲基氯化铵(Arquad 2C-75〜R)和PMMA试样的水凝胶。在主要沉降之前以交错的间隔(2、4和6周)部署了三个面板苏格兰克莱德峡湾的半巴拉米纳德斯巴拉诺德氏菌和可食用的Mytilus紫罗兰季,分别放置了10、12和14周,结果表明没有样品能完全抵抗结垢,但是Arquad 2C-75〜R水凝胶非常耐污染尽管最初的亲水性有所不同,但最重的污垢物质是未加载的水凝胶和PMMA,有效防止了微污垢和大污垢。 2C-75〜R水凝胶在防止幼虫沉降方面同样有效,长达14周。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号