首页> 外文期刊>Applied Surface Science >Determination of corrosion protection current density requirement of zinc sacrificial anode for corrosion protection of AA5083-H321 in seawater
【24h】

Determination of corrosion protection current density requirement of zinc sacrificial anode for corrosion protection of AA5083-H321 in seawater

机译:锌牺牲阳极腐蚀保护电流密度要求在海水中AA5083-H321腐蚀保护的腐蚀保护电流密度要求

获取原文
获取原文并翻译 | 示例

摘要

In this study, the current density requirements of zinc sacrificial anode for corrosion protection of AA5083-H321 aluminum hull for the ship was determined through various electrochemical tests. Surface observation and chemical composition analysis were performed after the galvanostatic test for various current density requirements determined by the cathodic polarization experiment. As a result, the most appropriate current density requirement range was determined as 3.7 x 10(-6)-5.8 x 10(-6) A/cm(2). Excessive current density over 7.6 x 10(-6) A/cm(2) caused local surface damage due to the effect of Mg-rich and Fe-rich intermetallic phases. In addition, the self-consumption of zinc sacrificial anode was determined through Tafel's extrapolation method.
机译:在该研究中,通过各种电化学测试确定了用于船舶AA5083-H321铝壳体腐蚀保护的锌牺牲阳极的电流密度要求。在通过阴极偏振实验确定的各种电流密度要求的电流测试之后进行表面观察和化学成分分析。结果,最合适的电流密度要求范围确定为3.7×10( - 6)-5.8×10(-6)A / cm(2)。电流密度超过7.6×10(-6)A / cm(2)由于富含Mg的金属间相阶段的效果导致局部表面损伤。此外,通过Tafel的外推法测定锌牺牲阳极的自消耗。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号