Testing of a cryocooler-cooled HTS magnet with silver-sheathed Bi2223 tapes for silicon single-crystal growth applications

机译:带有银护套Bi2223胶带的低温冷却器高温超导磁体的测试,用于硅单晶生长应用

获取原文
获取原文并翻译 | 示例

摘要

A project to develop a high-temperature superconducting split magnet for 8 inch silicon single-crystal growth applications began in October 1997. This split coil system is composed of 2 coils, each consisting of 18 pancakes. Each coil has an outer diameter of 1.2 m and a thickness of 0.1 m. Moreover, we developed a highly efficient GM-type cryocooler to cool a HTS coil to below 20 K. This paper presents the test results for a full-scale magnet. Each coil was cooled by the GM-cryocooler with a 3.3 kW compressor. The cool-down of the coil was completed within 480 hours with temperature difference among pancakes maintained at less than 18 K. In April 2001 this split coil was successfully energized up to rated current of 210 A at 20 K without a quench. The stored energy of this split coil reached 1.1 MJ at 216 A, 20 K, and the fastest charging time in our experiments was 1 minute.
机译:1997年10月开始了一个开发用于8英寸硅单晶生长应用的高温超导分裂磁体的项目。该分裂线圈系统由2个线圈组成,每个线圈由18个煎饼组成。每个线圈的外径为1.2 m,厚度为0.1 m。此外,我们开发了一种高效的GM型低温冷却器,可将HTS线圈冷却至20 K以下。本文介绍了全尺寸磁体的测试结果。每个线圈均由带有3.3 kW压缩机的GM低温冷却器进行冷却。线圈的冷却在480小时内完成,煎饼之间的温差保持在18 K以下。2001年4月,该分流线圈在20 K时成功通电,额定电流为210 A,没有淬火。在216 A,20 K时,该分流线圈的存储能量达到1.1 MJ,在我们的实验中最快的充电时间是1分钟。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号