PURPOSEOne of the most important factors in evaluating the quality of fixed dental prostheses (FDPs) is their gap. The purpose of this study was to compare the marginal and internal gap of two different metal-ceramic crowns, casting and selective laser sintering (SLS), before and after porcelain firing. Furthermore, this study evaluated whether metal-ceramic crowns made using the SLS have the same clinical acceptability as crowns made by the traditional casting.
机译:目的评估固定牙修复体(FDP)质量的最重要因素之一是它们的差距。这项研究的目的是比较两种不同的金属陶瓷冠,在烧制前后的边缘和内部间隙,分别是铸造法和选择性激光烧结法(SLS)。此外,本研究评估了使用SLS制成的金属陶瓷冠与传统铸件制成的冠具有相同的临床可接受性。