PURPOSE One of the most important factors in evaluating the quality of fixed dental prostheses (FDPs) is their gap. The purpose of this study was to compare the marginal and internal gap of two different metal-ceramic crowns, casting and selective laser sintering (SLS), before and after porcelain firing. Furthermore, this study evaluated whether metal-ceramic crowns made using the SLS have the same clinical acceptability as crowns made by the traditional casting. MATERIALS AND METHODS The 10 study models were produced using stone. The 20 specimens were produced using the casting and the SLS methods; 10 samples were made in each group. After the core gap measurements, 10 metal-ceramic crowns in each group were finished using the conventional technique of firing porcelain. The gap of the metal-ceramic crowns was measured. The marginal and internal gaps were measured by two-dimensional and three-dimensional replica techniques, respectively. The Wilcoxon signed-rank test, the Wilcoxon rank-sum test and nonparametric ANCOVA were used for statistical analysis (α=.05). RESULTS In both groups, the gap increased after completion of the metal-ceramic crown compared to the core. In all measured areas, the gap of the metal cores and metal-ceramic crowns produced by the SLS was greater than that of the metal cores and metal-ceramic crowns produced using the casting. Statistically significant differences were found between cast and SLS (metal cores and metal-ceramic crown). CONCLUSION Although the gap of the FDPs produced by the SLS was greater than that of the FDPs produced by the conventional casting in all measured areas, none exceeded the clinically acceptable range.
机译:目的评估固定义齿(FDP)质量的最重要因素之一是它们的间隙。这项研究的目的是比较两种不同的金属陶瓷冠,在烧制前后的边缘和内部间隙,分别是铸造和选择性激光烧结(SLS)。此外,这项研究评估了使用SLS制成的金属陶瓷冠与传统铸件制成的冠在临床上是否具有相同的可接受性。材料与方法10种研究模型是用石材制成的。使用浇铸和SLS方法生产了20个试样。每组制作10个样品。在芯间隙测量之后,使用常规的烧瓷技术完成每组中的10个金属陶瓷冠。测量金属陶瓷冠的间隙。边缘和内部间隙分别通过二维和三维复制技术进行测量。使用Wilcoxon符号秩检验,Wilcoxon秩和检验和非参数ANCOVA进行统计分析(α= .05)。结果在两组中,与芯相比,金属陶瓷冠完成后间隙增大。在所有测量区域中,由SLS产生的金属芯和金属陶瓷冠的间隙大于使用铸件产生的金属芯和金属陶瓷冠的间隙。在铸造和SLS(金属芯和金属陶瓷冠)之间发现了统计学上的显着差异。结论尽管在所有测量区域中SLS产生的FDP的间隙均大于常规铸造产生的FDP的间隙,但均未超出临床可接受的范围。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号