A series of corrosion problems caused by high-temperature, high-pressure and high-acid gas environments has been an issue in oil and gas production for a long time. During the development of a high-acid gas field, the petroleum pipe is subjected to many aspects of corrosion, and the corrosion mechanism is complicated by the condition of the coexistence of H2S/CO2. Based on the study of the corrosion problem associated with the formate packer fluid in Southwest China, three kinds of steels were studied for corrosion prevention in the alloy G3/N80 steel/TP110SS steel. The study shows that the corrosion rate of the formate packer fluid is low, but corrosion is severe in environments characterized by high temperatures, high pressures and high-acid gas contents. Based on the consideration of cost and the difficulty of realization, an anti-corrosion system was constructed based on the existing packer fluid, mainly through the introduction of a variety of anti-corrosion additives. Through the selection of various additives and corrosion experiments, a corrosion protection system of formate packer fluid was developed. Corrosion tests show that the corrosion rate of the system must be less than 0.076 mm yr−1 to achieve the purpose of corrosion protection. The formate packer fluid with corrosion protection can meet the needs of the current application.
机译:长期以来,由高温,高压和高酸性气体环境引起的一系列腐蚀问题一直是油气生产中的问题。在高酸性气田开发过程中,石油管道受到许多方面的腐蚀,并且由于H2S / CO2的共存条件,腐蚀机理变得复杂。在研究西南地区与甲酸封隔器流体有关的腐蚀问题的基础上,研究了三种合金G3 / N80钢/ TP110SS钢的防腐蚀性能。研究表明,甲酸封隔器液体的腐蚀速率较低,但在以高温,高压和高酸性气体含量为特征的环境中腐蚀严重。在考虑成本和实现难度的基础上,主要通过引入多种防腐添加剂,在现有的封隔液基础上构建了防腐系统。通过选择各种添加剂和腐蚀实验,开发了甲酸酯封隔液的腐蚀防护系统。腐蚀试验表明,系统的腐蚀速率必须小于0.076 mm yr -1 才能达到防腐蚀的目的。具有防腐功能的甲酸酯封隔器流体可以满足当前应用的需求。