摘要

采用永磁强磁选-酸浸工艺对普通级石英砂进行排杂提纯实验,研究了矿粉细度、磁感应强度、酸液浓度和浸泡时间对石英砂提纯效果的影响,从而得到提纯效果最佳的条件参数。结果表明:矿粉细度和磁感应强度是石英砂磁选的主要影响因素,磁选后石英砂SiO2纯度可达到99.9%,Fe含量为0.013%;常温下,酸液浓度和浸泡时间是石英砂酸浸的主要影响因素,酸浸后石英砂SiO2纯度可达到99.99%,Fe含量为0.0004%,经该工艺处理后的石英砂已达到超高纯石英砂级别。%General level silica sand was puriifed by permanent strong magnetic separation and acid leaching. Effects of slag ifneness, magnetic ifeld intensity, acid concentration and immersion time on silica sand puriifcation were studied to obtain the best conditional parameters. The results show that particle size and magnetic ifeld intensity are main factors in effecting the magnetic separation of silica sand. SiO2 purity can reach 99.9%and Fe content is 0.013%after dry magnetic separation. At room temperature, acid concentration and immersion time are main factors in effecting the acid leaching of silica sand. SiO2 purity can reach 99.99%and Fe content is 0.0004%after acid leaching. After this process, silica sand has reached the ultra-pure level.

著录项

  • 来源
    《非金属矿》 |2015年第3期|52-54|共3页
  • 作者

    王华庆; 张树光; 李江山;

  • 作者单位

    辽宁工程技术大学 土木与交通学院;

    辽宁 阜新 123000;

    中国科学院武汉岩土力学研究所;

    湖北 武汉 430000;

    辽宁工程技术大学 土木与交通学院;

    辽宁 阜新 123000;

    中国科学院武汉岩土力学研究所;

    湖北 武汉 430000;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 TD973+.3;
  • 关键词

    石英砂; 永磁强磁选; 酸浸; 提纯;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号