摘要

四川西部地区某含铜铁矿石中铁主要以鲕状赤铁矿形式存在,铜主要以结合氧化铜形式存在.对该矿石进行了氯化离析一浮选一弱磁选试验,结果表明:将矿石在氯化钠和焦炭用量均为7%、离析温度为950℃、离析时间为60min的条件下进行氯化离析焙烧后,经1粗2精3次浮选,可以得到铜品位为19.64%、铜回收率为82.41%的铜精矿,浮选尾矿经1次弱磁选,可以得到铁品位为65.86%、铁回收率为78.62%的铁精矿.%Iron minerals in a copper-iron ore in the region of western Sichuan mainly exists in form of oolitic hematite,and copper is mainly associated with copper oxide, so the process of chlorination segregation -flotation-low intensity magnetic separation was adopted for this ore. The results showed that under conditions of sodium chloride and coke dosage of 7% respectively, segregation temperature at 950 ℃ for 60 min, following by chlorination segregation and roasting, copper concentrate with Cu grade of 19. 64%, and Fe recovery of 82. 41% were obtained by the process of one ronghing-two cleaning flotation. Then for tailings, iron concentrate with Fe grade of 65.86%, and Fe recovery of 78. 62% were obtained by one low intensity magnetic separation.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号