摘要

嵌布粒度不同的鳞片石墨浮选性质也有所差异,针对甘肃民勤鳞片石墨矿(1#矿)和黑龙江萝北鳞片石墨矿(2#矿)两种不同嵌布粒度的鳞片石墨矿石分别进行了矿石性质及浮选速率研究.研究表明,2#矿的石墨鳞片大于1#矿样;2#矿的浮选速率常数较1#矿高;随着煤油用量的增加,且浮选速率常数均逐渐升高后趋于平缓,浮选速率常数最大值分别为1.344 min-1和3.036 min-1;随着2#油用量的增加,精矿固定碳含量均逐渐降低后有小幅上升.试验表明可通过控制浮选时间,适量增加煤油用量,降低2#油用量达到提前回收部分石墨鳞片的目的.%The flake graphite with different dissemination size has different flotation properties.The research on Minqin flake graphite mine (1#) and Luobei flake graphite mine (2#) of ore properties and flotation rate were carried out.The graphite scale of 2# graphite was larger than 1#.The research of flotation rate demonstrated that flotation rate flotation rate constant increased with the amount of kerosene,the maximum constant is 1.34 min-1 and 3.04 min-1,fixed carbon content decreased first and then increased with the increase of the amount of terpene oil,the constant of 2# graphite was higher than 1#.The purpose of retrieving part of graphite flake in advance could be achieved by means of controlling scraping time,increasing amount of kerosene,reducing amount of terpene oil.

著录项

  • 来源
    《中国矿业》 |2017年第7期|116-120,128|共6页
  • 作者单位

    武汉理工大学资源与环境工程学院,湖北 武汉 430070;

    武汉理工大学资源与环境工程学院,湖北 武汉 430070;

    武汉理工大学矿物资源加工与环境湖北省重点实验室,湖北 武汉 430070;

    武汉理工大学资源与环境工程学院,湖北 武汉 430070;

    武汉理工大学矿物资源加工与环境湖北省重点实验室,湖北 武汉 430070;

    武汉理工大学资源与环境工程学院,湖北 武汉 430070;

    武汉理工大学矿物资源加工与环境湖北省重点实验室,湖北 武汉 430070;

    武汉理工大学资源与环境工程学院,湖北 武汉 430070;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 非金属矿选矿;
  • 关键词

    鳞片石墨; 嵌布粒度; 浮选速率;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号