Analysis and discussion on the surface linear defect of cold-rolling sheet steel

机译:冷轧钢板表面线性缺陷的分析与讨论

获取原文

摘要

A series of surface linear defects of cold-rolling sheet steel have been investigated by Scanning Electron Microscope (SEM) and X-ray Energy Dispersive Spectrometry(EDS).The results show that a lot of inclusions, gas holes and some feature of free surface like spore exist behind or on the defects, and a lot of bigger nonmetallic inclusions have the same composition as the hot-rolling steel plate, by means of simulation figure, it is described that the inclusions (or gas holes) within the slab could expose upon the surface of sheet steel after hot-rolling and cold-rolling, and finally become the linear surface defects whose appearance are bubble, crumple and darking-down. Meanwhile, it's regarded that the amount, size and shape of the nonmetallic inclusions (or remant gas holes) within the slab are a very important affecting factor on the surface quality of cold-rolling sheet steel, although they could not do harm to the surface quality of hot-rolling steel products.
机译:利用扫描电子显微镜(SEM)和X射线能谱仪(EDS)对冷轧钢板的一系列表面线性缺陷进行了研究,结果显示出大量的夹杂物,气孔和一些自由表面特征像是孢子存在于缺陷的后方或缺陷上,并且许多较大的非金属夹杂物与热轧钢板具有相同的成分,通过模拟图可知,板坯中的夹杂物(或气孔)可能暴露在外。在热轧和冷轧后的薄钢板表面上,最终成为外观呈气泡,起皱和变暗的线性表面缺陷。同时,认为板坯中的非金属夹杂物(或残留的气孔)的数量,大小和形状是对冷轧钢板表面质量的重要影响因素,尽管它们对表面无害。热轧钢产品质量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号