【24h】

Making Alumina Microcomponents From Al Powder

机译:由铝粉制造氧化铝微组分

获取原文
获取原文并翻译 | 示例

摘要

Alumina microcomponents have distinguishing advantages over Si counterparts. However, the shrinkage of alumina, as high as 20%, makes it difficult to produce precision components that require a high tolerance. A new fabrication process is presented to greatly reduce the shrinkage. The process consists of forming an Al powdered component through sintering and transforming the Al powdered component into an alumina part. In this way, the shrinkage occurring in sintering the Al powder component will be compensated by the expansion occurred when Al transforms into alumina. The process involves producing micro-moulds, preparing metallic paste, filling the micro-moulds with the metallic paste, demoulding, sintering the green Al patterns and finally oxidising the sintered Al-based components to achieve alumina components. The process was proven successful. Characterization of the sintered alumina microcomponents has been undertaken, including SEM image analysis, density and scale measurements.
机译:氧化铝微组分比硅对应物具有明显的优势。但是,氧化铝的收缩率高达20%,使得难以生产需要高公差的精密部件。提出了一种新的制造工艺以大大减少收缩。该方法包括通过烧结形成铝粉成分并将该铝粉成分转化为氧化铝部件。这样,在烧结Al粉末组分时发生的收缩将被当Al转变成氧化铝时发生的膨胀所补偿。该过程涉及生产微模具,制备金属浆料,用金属浆料填充微模具,脱模,烧结生铝图案,最后氧化烧结的铝基成分以制成氧化铝成分。该过程被证明是成功的。已经对烧结的氧化铝微组分进行了表征,包括SEM图像分析,密度和水垢测量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号