The ultrafine, monodispersed, spherical cobalt powder has been fabricated by reducing cobalt hydroxide with glycol. It were investigated that the effect of NaOH concentration on the reaction rate and the effects of the concentration of cobalt hydroxide and surfactant on the morphology and particle size. The particles were characterized by the X-ray diffraction(XRD), scanning electron microscope(SEM), laser diffraction particle size analyzer and BET specific surface analyzer respectively. The XRD shows that the cobalt powders exist mostly in face centered cubic (fcc) structure, a little in simple hexagonal. The cobalt powders prepared at Co(OH)_2 150g/L, NaOH 40 g/L and surfactant 30g/L, its average particle size, specific surface area and cobalt content, were 0.88μm, 2.705m~2/g. and more than 99.5% respectively.
机译:超细的单分散球形钴粉是通过用乙二醇还原氢氧化钴制成的。研究了NaOH浓度对反应速率的影响以及氢氧化钴和表面活性剂的浓度对形态和粒度的影响。分别通过X射线衍射(XRD),扫描电子显微镜(SEM),激光衍射粒度分析仪和BET比表面分析仪对其进行表征。 X射线衍射表明,钴粉主要以面心立方(fcc)结构形式存在,而很少以简单的六角形形式存在。 Co(OH)_2为150g / L,NaOH为40g / L,表面活性剂为30g / L时制备的钴粉,其平均粒径,比表面积和钴含量分别为0.88μm,2.705m〜2 / g。和分别超过99.5%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号