Metal-organic deposition with low fluorine content precursor solution (LF-MOD) can be used for large-scale fabrication of YBCO coated conductor with advantage of reducing the long fabrication period compared to traditional TFA-MOD. In this paper 5-layer YBCO films were prepared with thickness over 2.5μm by LF-MOD. And then the effect of high-temperature annealing time of 2h, 4h, 6h, respectively on the morphology and texture of YBCO films were systematically investigated. The results show that film of 6h annealing performs best.
机译:具有低氟含量前体溶液(LF-MOD)的金属有机沉积可用于YBCO涂覆导体的大规模制造,其有利于减少与传统TFA-MOD相比的长制造周期。在本文中,通过LF-mod厚度超过2.5μm的厚度制备5层YBCO膜。然后系统地研究了高温退火时间为2h,4h,6h的效果,分别对Ybco薄膜的形态和质地进行了系统地进行了系统地研究。结果表明,6H退火的胶片表现最佳。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号