The present study deals with investigations relating to dry sliding wear behaviour of the Al 7075 alloy, reinforced with Al2O3 and B4C. The hybrid composites are produced through Liquid Metallurgy route - Stir casting method. The amount of Al2O3 particles is varied as 3, 6, 9, 12 and 15 wt% and the amount of B4C is kept constant as 3wt%. Experiments were conducted based on the plan of experiments generated through Taguchi's technique. A L27 Orthogonal array was selected for analysis of the data. The investigation is to find the effect of applied load, sliding speed and sliding distance on wear rate and Coefficient of Friction (COF) of the hybrid Al7075-Al2O3-B4C composite and to determine the optimal parameters for obtaining minimum wear rate. The samples were examined using scanning electronic microscopy after wear testing and analyzed.
机译:本研究涉及与Al 7075合金的干滑动磨损行为有关的研究,用Al2O3和B4C加固。通过液态冶金型液搅拌铸造方法生产混合复合材料。 Al 2 O 3颗粒的量随5,6,9,12和15wt%而变化,B4C的量保持恒定为3wt%。基于通过Taguchi技术产生的实验计划进行实验。选择L27正交阵列以分析数据。调查是为了找到杂交AL7075-AL2O3-B4C复合材料的磨损,滑动速度和滑动距离磨损率和摩擦系数(COF)的影响,并确定获得最小磨损率的最佳参数。在磨损测试后使用扫描电子显微镜检查样品并分析。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号