首页> 外文会议>International Conference on Engineering, Science and Technology >The utilization of stone ash on cellular lightweight concrete
【24h】

The utilization of stone ash on cellular lightweight concrete

机译:采用石灰在蜂窝轻质混凝土上的利用

获取原文

摘要

Lightweight concrete brick is a brick which made of cement, sand, water, and foam as the basic composition. This brick are divided into 2, based on the foam used such as AAC (Autoclave Aerated Concrete) that use aluminium paste and CLC(Cellular Lightweight Concrete) that use foaming agent from BASF as its foaming material. In this trial, the lightweight brick that are ging to be use are the CLC with foaming agent as its foaming material with the mixture of stone ash that are produced by the Stone Crusher with spesific gravity 2666 kg/m~3 as their partly sand substitution . In this research, the stone ash variant that are used are 10%, 15%, and 20% from the amount of sand that planned before. After casting, the result of the 10% will receive a reduction of compressive strength while an increasing in absorption as 25.07% and 39.005% and the 15% variant will recieve a reduction of compressive strength as much as 65.8% and a reduction of absorption as much as 17.441% and the 20% variant will recieve a reduction of compressive strength as much as 67.4% while an increasing of absorption as much as 17.956%.
机译:轻质混凝土砖是由水泥,沙子,水和泡沫为基本成分的一块砖。此砖分为2,基于所述泡沫材料中使用诸如AAC(蒸压加气混凝土)的在使用铝浆和CLC(蜂窝轻质混凝土)的在使用来自BASF发泡剂作为其发泡材料。在该试验中,被吉宁轻质砖是使用与发泡剂作为与由石破碎机产生具有spesific重力2666公斤/米〜3作为其部分地砂取代石灰的混合物其发泡性材料的CLC 。在这项研究中,所使用的石灰渣变型是10%,15%,从之前计划的沙量的20%。铸造后,将10%的结果将获得的降低的压缩强度,而一个在吸收为25.07%和39.005%增加,15%的变体将收到的降低的压缩强度高达65.8%和作为还原吸收的高达17.441%和20%的变体将收到的降低的压缩强度高达67.4%,而一个尽可能多的吸收增加为17.956%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号