Brine leaching of a TSL processed zinc-plant residue (ZPR), containing 83.3% anglesite, has been investigated for lead recovery. A prior treatment of ZPR in acid solution did not show any significant effect of acid concentration in zinc dissolution. The study reveals that the solubility limits of PbCl_2 is as an important factor with respect to the brine concentration and pulp density in lixiviant. The dissociated sulfate ions hinder the formation of PbCl_2 on prolong leaching (above 60 min), while exhibiting the reverse solubility of lead as PbSO_4. A 3-step leaching process could yield >92% leaching efficiency when the parameters were maintained as: 10% pulp density in a 250 g/L NaCl solution, 80 °C temperature, and 60 min time. This leaves the insoluble ferrite, sulfides and oxy-sulfates of zinc and lead in the final residue as revealed by the XRD characterization.
机译:已经研究了含有83.3%的角度的TSL加工锌 - 植物残基(ZPR)的盐水浸出,以进行铅回收率。在酸溶液中对ZPR的先前治疗没有显示出锌溶解中的酸浓度的任何显着影响。该研究表明,PbCl_2的溶解度限制是关于Lixiviant中盐水浓度和纸浆密度的重要因素。解离的硫酸酯离子妨碍延长浸出(高于60分钟)的PbCl_2,同时表现出铅的逆转溶解度作为PBSO_4。当将参数维持为:250g / L NaCl溶液,80℃温度和60分钟时间,3步浸出过程可以产生> 92%的浸出效率。这使得锌的不溶性铁氧体,硫化物和氧硫酸盐,并在XRD表征揭示的最终残留物中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号