Orthogonal array design (OAD) has been used to arrange the experimental runs in order to maximize lead recovery and also minimize zinc dissolution from an Iranian zinc plant residue (ZPR). The residue assaying 9.21 percnet Zn, 12.37 percnet Pb and 5.31 percnet Fe was used in successive processes involving sulfuric acid (H_2SO_4)-water leaching to bring zinc into solution and therefore enrich the lead in the residue and then brine leaching for lead recovery. An L_(25) orthogonal array (OA, five factors in five levels) was employed to evaluate the effects of NaCl concentration (C_(brine)=50,150, 200, 250, 300 g/L), time (t=10, 20, 30, 40 and 50 min), pulp density (S/L=25, 50,100,150 and 200 g/L), pH (1,2,3,4,5) and stirring speed (R=100,200,300,400 and 500 rpm) on extraction of the individual metal ions (Pb, Zn, Fe). Statistical analysis, ANOVA, was also employed to determine the relationship between experimental conditions and yield levels. The results showed that increasing pulp density and initial pH reduced mean responses for lead. However, increasing brine concentration promoted the recovery of lead. The experimental results for selective leaching showed that under optimal leaching conditions (S/L)_1: 25 g/L, (pH)_1:1, t_3:30 min, (C_(brine))_5: 300 g/Land R_4:400 rpm, the extraction of lead and zinc were 89.43 percnet and 3.84 percnet, respectively; giving a solution containing 2.99 g/L Pb, 0.02 g/L Zn and negligible amount of iron.
机译:正交阵列设计(OAD)已用于安排实验运行,以使铅的回收率最大化,并使锌从伊朗锌厂残渣(ZPR)中的溶解最小化。残留物含量测定为9.21 percnet Zn,12.37 percnet Pb和5.31 percnet Fe,可用于随后的过程,包括硫酸(H_2SO_4)-水浸出以将锌引入溶液中,从而使残留物中的铅富集,然后进行盐水浸出以回收铅。使用L_(25)正交阵列(OA,在五个级别中的五个因子)评估NaCl浓度(C_(盐水)= 50,150,200,250,300 g / L),时间(t = 10,20 ,30、40和50分钟),纸浆密度(S / L = 25、50,100,150和200 g / L),pH(1,2,3,4,5)和搅拌速度(R = 100,200,300,400和500 rpm)提取单个金属离子(Pb,Zn,Fe)。统计分析,方差分析,也被用来确定实验条件和产量水平之间的关系。结果表明,增加纸浆密度和初始pH值会降低铅的平均响应。但是,盐水浓度的增加促进了铅的回收。选择性浸出的实验结果表明,在最佳浸出条件下(S / L)_1:25 g / L,(pH)_1:1,t_3:30 min,(C_(盐水))_ 5:300 g / L,R_4: 400 rpm时,铅和锌的提取率分别为89.43 percnet和3.84 percnet。得到含有2.99 g / L Pb,0.02 g / L Zn和微量铁的溶液。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号