首页> 外国专利> HYDROMETALLURGICAL PROCESS FOR THE RECOVERY OF LEAD, SILVER, GOLD AND ZINC FROM IMPURE JAROSITE RESIDUES OF AN ELECTROLYTIC ZINC PROCESS

HYDROMETALLURGICAL PROCESS FOR THE RECOVERY OF LEAD, SILVER, GOLD AND ZINC FROM IMPURE JAROSITE RESIDUES OF AN ELECTROLYTIC ZINC PROCESS

机译:从电解锌工艺的纯铁水残渣中回收铅,银,金和锌的水热法

摘要

A HYDROMETALLURGICAL PROCESS FOR THE RECOVERY OF LEAD, SILVER AND GOLD, AS WELLAS ZINC, FROM IMPURE JAROSITE RESIDUES OF AN ELECTROLYTIC ZINC PROCESSABSTRACT OF THE DISCLOSUREThe impure jarosite residue of an electrolytic zinc process is leached in asulfuric-acid-bearing solution in order to produce a leach residue which con-tains lea?, silver and gold and a ferrisulfate-bearing solution and to separatethem from each other, whereafter the leach residue is sulfidized and froth-flotated in order to recover a combined concentrate which contains lead, silverand gold, and the ferrisulfate-bearing solution is fed to a ferritic treatmentstage, in which ferrisulfate and ferrites react in the presence of ions ofalkali and ammonium at 80-105°C and form pure jarosite and zinc sulfate.
机译:铅,银和金以及其他材料的水热回收工艺作为锌,来自电解锌工艺的不纯亚铁酸盐残渣披露摘要电解锌过程中不纯的黄钾铁矾残留物在含硫酸溶液以产生浸出残渣含有lea ?、银和金以及一种含硫酸铁的溶液,并进行分离它们彼此分离,然后浸出残渣被硫化并起泡-浮选以回收包含铅,银的混合精矿和金,然后将含硫酸铁的溶液送入铁素体处理阶段,其中硫酸亚铁和铁氧体在离子的存在下反应在80-105°C下与碱和铵形成碱性,形成纯黄钾铁矾和硫酸锌。

著录项

  • 公开/公告号CA1181598A

    专利类型

  • 公开/公告日1985-01-29

    原文格式PDF

  • 申请/专利权人 OUTOKUMPU OY SF-83500 OUTOKUMPU;

    申请/专利号CA19810387013

  • 发明设计人 NYBERG JENS R.;RASTAS JUSSI K.;

    申请日1981-09-30

  • 分类号C22B11/04;C22B13/04;C22B19/22;

  • 国家 CA

  • 入库时间 2022-08-22 08:05:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号