Gas temperatures can reach almost 1000°C Cells casings don't always fail at vent Failure can propagate to another cell at least 32 mm away in somewhat open environment More gas is released for NCR18650B than cells tested in published literature Ejecta from cell can include not just ash, but large pieces of metal electrodes PTC fuses may fail as cell temperature is increased.
机译:气体温度可达到近1000°C细胞外壳并不总是在通气故障时失效,可以传播到另一个电池在稍微开放的环境中至少32毫米,对于NCR18650B的释放比在来自细胞的公开文献喷射物中释放出更多的气体可以包括不包括 只需灰,但大块金属电极PTC熔丝可能由于细胞温度而失效。