首页> 外文会议>Annual International Conference Battery Safety >Destructive Testing of Lithium Ion Cells
【24h】

Destructive Testing of Lithium Ion Cells

机译:锂离子细胞的破坏性测试

获取原文

摘要

Gas temperatures can reach almost 1000°C Cells casings don't always fail at vent Failure can propagate to another cell at least 32 mm away in somewhat open environment More gas is released for NCR18650B than cells tested in published literature Ejecta from cell can include not just ash, but large pieces of metal electrodes PTC fuses may fail as cell temperature is increased.
机译:气温可达到近1000°C的细胞外壳并不总是在排气口失效的情况下不能宣传到另一个电池至少32mm的距离在稍微开放的环境中,对于在来自细胞的公开文献喷射物中释放的NCR18650B的细胞可以包括不包括只需灰,但大块金属电极PTC保险丝可能由于细胞温度增加而失效。