The corrosion rates of rebar HRB335 in 0.5%wt. NaCl solution and the tensile mechanical properties before and after corrosion of rebar were investigated. The results showed that, with increasing corrosion time from 30 days to 90 days, the corrosion rate of rebar HRB335 increases. With the increase of corrosion time (corrosion rate), the yield strength and tensile strength decrease, but the elongation decreases at first and then increases.
机译:螺旋HRB335的腐蚀速率为0.5%wt。研究了螺纹钢腐蚀前后的NaCl溶液和拉伸机械性能。结果表明,随着30天至90天的腐蚀时间的增加,钢筋HRB335的腐蚀速率增加。随着腐蚀时间(腐蚀速率)的增加,屈服强度和拉伸强度降低,但是伸长率先降低,然后增加。