Decay Degree determination of Archaeological Shell Objects from the Great Temple of Tenochtitlan, using a Visible Light Spectrometer

机译:衰变度测定租用光谱仪从Tenochtitlan的大寺庙中考古壳体的测定

获取原文

摘要

In four offerings of the Great Temple of Tenochtitlan five groupings of Pinctada Mazatlanica shell pendants were found. Due to the burial conditions, damages on the surfaces can be observed in almost all the objects. In order to assess the deterioration degree, we used a visible light spectrometer. This is an inexpensive method to determine qualitatively the reflectance of the light at the surface that is directly related to the amount of organic material remains in these objects. This data may be used as a conservation marker for monitoring the collection and it can provide outstanding information to preserve the fragile shell pendants using a non-destructive method.
机译:在Tenochtitlan的伟大寺庙的四个产品中,发现了五个山茱萸渣壳吊坠。由于埋葬条件,可以在几乎所有物体中观察到表面上的损坏。为了评估劣化程度,我们使用了可见光谱仪。这是一种廉价的方法,可以确定地确定与有机材料的量直接相关的光的光的反射率保留在这些物体中。该数据可以用作保护标记,用于监视集合,并且可以使用非破坏方法提供优异的信息来保护脆弱的外壳吊坠。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号