Contrastive analysis on low temperature carbonization of longkou and yaojie oil shale in aluminum retort

机译:铝蒸馏中龙口和瑶家油页岩低温碳化对比分析

获取原文

摘要

Lots of basic analyses carried on YJOS (Yaojie oil shale) and LKOS (Longkou oil shale) consist of proximate analysis, ultimate analysis, XRF analysis and shale oil yield in aluminum retort. Besides, TGA are used on YJOS, LKOS and shale oil, gas chromatographic analysis is used on retorting gas. The results show that LKOS and YJOS have the same hydrogen-to-carbon ratio, but LKOS has higher volatile component and its oil yield in aluminum retort is much higher than YJOS. Ca content in LKOS is much higher than YJOS, however, Al and Fe content in LKOS are lower than YJOS. Two kinds of shale oil after destructive distillation have similar composition and relative content, in addition, they all produce more low boiling point distillates, combustible component of their destructive distillation gas are H_2 and CH4, the second are CO and C_2H_6. Aluminium retort experimental findings, The carbonization temperature is the main influence factor on oil shale destructive distillation process in aluminum retort. Residence time has small influence on shale oil yield but need to choose appropriate heating rate and particle size. Best carbonization parameters of LKOS in aluminum retort: Temperature 500-550°C, heating rate 5°C/min, particle size 2~4mm, Residence time 10~20min; the best parameters of YJOS: Temperature 500~550°C, heating rate 5°C/min, particle size0.2-0.9mm, residence time 10-20min.
机译:在YJOS(雅杰油页岩)和LKOS(龙口石油页岩)上进行了许多基本分析包括替代分析,终极分析,XRF分析和铝蒸馏的页岩油产量。此外,TGA用于YJOS,LKOS和页岩油,气相色谱分析用于蒸馏气。结果表明,LKOS和YJO具有相同的氢气与碳比,但LKOS具有较高的挥发性组分,其铝蒸馏中的油产量远高于YJO。 LKO中的CA含量远高于YJO,然而,LKO中的Al和Fe含量低于YJO。破坏性蒸馏后两种页岩油具有相似的组成和相对含量,此外,它们都产生更低的沸点馏分,其破坏性蒸馏气体的可燃组分是H_2和CH4,第二是CO和C_2H_6。铝蒸馏实验结果,碳化温度是铝蒸馏中油页岩破坏蒸馏工艺的主要影响因素。停留时间对页岩油产生的影响很小,但需要选择适当的加热速率和粒度。最佳碳化参数在铝蒸煮器中的液体:温度500-550°C,加热速率5°C / min,粒径2〜4mm,停留时间10〜20min; YJOS的最佳参数:温度500〜550°C,加热速率5°C / min,粒径0.2-0.9mm,停留时间10-20min。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号