In order to research the temperature-dropping characteristics of warm mix and hot mix asphalt, some rutting test panels are used as specimens to determine the temperature-dropping characteristics of hot mix asphalt(HMA), warm mix asphalt(WMA) with mixing additive "LuBo" and warm mix asphalt with mixing additive "Sasobit" under the conditions with initial temperatures of 110°C and 130°C. The test results indicate that: the higher initial temperature, the higher temperature-dropping rate is. After 25min the temperatures of rutting test panels with initial temperatures of 110°C and 130°C are close to 66°C and 68°C. The temperature-dropping rates of different types of mixtures are not the same. When the initial temperature is 110°C, the temperature-dropping rate of hot mix asphalt is the highest, the temperature-dropping rate of warm mix asphalt added with "Sasobit" is in the middle, and the temperature-dropping rate of warm mix asphalt added with "LuBo" is the lowest. After 35min, the temperatures of the three types of asphalt mixtures had fallen by 53°C, 51°C and 49°C separately.
机译:为了研究温热混合物和热混合物沥青的温度滴,一些车辙试验板用作试样,以确定热混合物沥青(HMA),温热混合沥青(WMA)的温度滴剂特性,与混合添加剂“ Lubo“和温热的沥青在初始温度为110℃和130°C的条件下混合添加剂”Sasobit“。测试结果表明:初始温度越高,较高的温度降低率是。 25分钟后,初始温度为110°C和130°C的车辙试验板的温度接近66°C和68°C。不同类型混合物的温度滴加速率不一样。当初始温度为110°C时,热混合沥青的温度滴加速率最高,温热混合沥青的温度滴加速率加入“索梭”在中间,温度滴加速度沥青添加了“Lubo”是最低的。 35分钟后,三种类型的沥青混合物的温度分别下降53℃,51℃和49℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号