Simulated leaching solution of tin anode slime was prepared as electrolyte to investigate the performance of cyclone electrowinning on extraction of tin from solution in this work. The results showed that Sn(II) could be extracted as sponge tin with cyclone electrowinning. Sn(IV) could be extracted as tin plate. As the concentration of tin chloride solution was lower, the current efficiency was lower and the quality of electrolytic product was poorer. On the condition of Sn(IV) concentration of 50 g/L, operation time of 2h, flow flux of 200 L/h and current density of 400 A/m~2, the current efficiency was more than 90% and the electrolytic product was of high purity which contains 99.5% tin. Cyclone electrowinning was proved to be an effective way to extract Tin from simulated leaching solution.
机译:制备锡阳极粘液的模拟浸出溶液作为电解质,以研究旋风电气宁对在这项工作中溶液中锡萃取的性能。结果表明,Sn(II)可以用旋风电绕组作为海绵锡提取。 Sn(iv)可以作为锡板提取。随着氯化锡溶液的浓度较低,电流效率较低,电解产物的质量较差。在Sn(iv)浓度为50g / l的条件下,操作时间为2h,流量通量为200升/小时,电流密度为400 a / m〜2,电流效率大于90%和电解产物纯度高,含有99.5%的锡。被证明是旋风电氢化是从模拟浸出溶液中提取锡的有效方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号